NCHRP Report 696: Performance of Corrugated Pipe Manufactured with Recycled Polyethylene Content (2011)
National Cooperative Highway Research Program (NCHRP)

Citation Manager

Thomas, Richard W, Cuttino, David, Transportation Research Board. "A.2.6 Percentage Polypropylene (TRI Method)." NCHRP Report 696: Performance of Corrugated Pipe Manufactured with Recycled Polyethylene Content. Washington, DC: The National Academies Press, 2011.

Please select a format:

BibTeX EndNote RefMan


Page
58
bottomleft bottomright
Page
58
Front Matter (R1-R11)
Summary (1-2)
Chapter 1 - Introduction (3-3)
Short-Term Properties (4-4)
Service Lifetime of PE (5-7)
The SIM for Predicting Creep and Creep Rupture (Stage I) Properties (8-11)
The FL-DOT Junction Test (12-12)
The Long-Term Oxidation (Stage III) Resistance (13-13)
Specifications (14-14)
Post-Industrial Recycled Polyethylene (15-15)
Post-Consumer Recycled High-Density Polyethylene (16-16)
PCR Mixed-Color Resin (17-17)
The Effects of Contamination (18-18)
The Effects of Melt Filtration (19-20)
The Effect of Silicone Rubber (21-23)
Phase 2 - Recycled-Resin Blends (24-25)
Blends Made with Mixed-Color PCR (26-27)
Blends Made with Natural PCR (28-29)
Blends Made with PIR-HD (30-31)
Index Test Results (32-33)
Stress-Crack Test Results (34-36)
Long-Term Tensile Strength by SIM (37-39)
Long-Term Creep Strain and Modulus by SIM (40-40)
Long-Term Stress-Crack Resistance (41-41)
Combined SIM (Stage I) and BFF (Stage II) Service-Lifetime Estimates (42-44)
The BFF Test for QC (45-45)
Designing Pipe with Recycled Content (46-46)
Proposed Draft Specifications (47-48)
Phase 2 - Recycled PE Blends (49-49)
Phase 3 - Pipe Made from Recycled-Resin Blends (50-53)
References (54-54)
Appendix A - Procedures and Test Methods (55-55)
A.2.4 Percentage Black/Color + Ash (ASTM D4218) (56-56)
A.2.6 Percentage Polypropylene (TRI Method) (57-58)
A.2.8 Flexural Modulus (ASTM D790) (59-59)
A.3.2 BAM Stress-Crack Test (TRI Method) (60-61)
A.3.3 BFF Test (TRI Method) (62-62)
A.3.4 Junction Test (FDOT FM 5-572) (63-63)
A.4.1 Stepped Isothermal Method (SIM) For Long-Term Creep Modulus and Strain (ASTM D6992) (64-64)
A.4.3 BFF Test for Long-Term Stress Crack Resistance (TRI Method) (65-68)
Appendix D - Pipe Containing Recycled HDPE (69-69)
Appendix E - Proposed Draft Standard Specification for PCR MCR High-Density PE Bottles for Use in AASHTO-Approved Corrugated Drainage Pipe (70-76)
Appendix F - Proposed Draft Standard for Recycled Content Containing HDPE Resin Formulations for Corrugated Pipe Made to AASHTO Standard M252-Recycled (77-84)
Appendix G - Proposed Draft Standard Specification for Recycled Content Containing HDPE Resin Formulations for Corrugated Pipe Made to AASHTO Standard M294-Recycled (85-93)
Appendix H - Proposed Draft Standard Specification for Corrugated Polyethylene Drainage Pipe Containing Recycled Polyethylene, 75- to 250-mm Diameter (94-108)
Appendix I - Proposed Draft Standard Specification for Corrugated Polyethylene Drainage Pipe Containing Recycled Polyethylene, 300- to 1,500-mm Diameter (109-129)
Abbreviations used without definitions in TRB publications (130-130)